WIDOCRYL-PG

WIDOCRYL-PG

Mixing

Before adding the components, WIDOCRYL-PG has to be stirred thoroughly. First, WIDOCRYL-SP Powder is added (mixing ratio: 1,5 kg powder : 1,0 kg WIDOCRYL-PG), followed by the hardener. The amount of hardener depends on the temperature. The dosage is stated on the lid. All components need to be mixed for at least 2 min. Due to the short pot life after the hardener has been added, we recommend to only mix small amounts.

Application

The finished mixture is poured on the surface. It can be spread using a rubber blade or a squeegee and then rolled off with a paint roller.

Quartz sand is then sprinkled into the wet WIDOCRYL-PG (approx. 4,5 kg/m², grain size 0,7 – 1,2 mm).

Further details, especially regarding hazard statements, security advices and measures in the event of fire can be found in the safety data sheet under sections 2, 4, 5, 6, 7 and 8.

Please also refer to our instructions on priming and to our technical information sheets!